Emissivity table (continue)
Material
Temperature°C
Emissivity
approximation
Iron
Polished cast iron
200
0.21
Processed cast iron
20
0.44
Polished tempered
iron
40250
0.28
Polished steel ingot
7701040
0.520.56
Raw welded steel
9451100
0.520.61
Surface ferric oxide
20
0.69
Completely rusty
surface
22
0.66
Rolled iron plate
100
0.74
Oxidized steel
198600
0.640.78
Cast iron (Oxidizing at
600°C )
198600
0.79
Steel (Oxidizing at
600°C )
125520
0.780.82
Electrolytic ferric
oxide
5001200
0.850.89
Iron plate
9251120
0.870.95
Cast iron, heavy ferric
oxide
25
0.80
Tempered iron, ferric
oxide
40250
0.95
Melting surface
22
0.94
Melting cast iron
13001400
0.29
Melting mild steel
16001800
0.28
Liquid steel
15001650
0.420.53
Pure liquid iron
15151680
0.420.45